Raw Ore: High-Silica Phosphate Ore
P2O5 Grade: 22%
SiO2 Content: 35%
Concentrate Grade: 31% P2O5, <8% SiO2
Recovery Rate: 82%
Capacity: 1500 tons per day
Work Scope: Engineering Design, Equipment Supply, Installation & Commissioning
Here are some photos of the project, click on the small picture to view the large picture.
Below are some ways to handle this plan. If you want to get a more detailed plan, please click the button to contact us.
Two-stage crushing system with jaw crusher and cone crusher
2-stage cleaner flotation with pH control to upgrade concentrate quality
Tailings thickener followed by paste plant for dry stack disposal
2-stage ball mill grinding in closed circuit with hydrocyclones to achieve target particle size of 74μm
Scavenger flotation to maximize recovery from rougher tailings
Process water recycling system for environmental compliance
To find out more about our products and solutions, please fll out the form below and one of our experts will get back to you shortly
3000 TPD Gold Flotation Project in Shandong Province
2500TPD Lithium Ore Flotation in Sichuan
Fax: (+86) 021-60870195
Address: No.2555,Xiupu Road, Pudong, Shanghai
Copyright © 2023. Prominer (Shanghai) Mining Technology Co.,Ltd.